SmCo Magnets – Samarium Cobalt Magnets

  • Manufactured using powder metallurgy processes from SmCo₅ or Sm₂Co₁₇ alloys
  • High resistance to demagnetization
  • Excellent corrosion resistance
  • Outstanding temperature stability
  • Relatively expensive due to limited raw material availability
  • Brittle and extremely hard

Typical Physical Properties

Curie Temperature (°C) 700-800
Maximum Operating Temperature (°C) 250 for SmCo5, 350 for Sm2Co17
Resistivity (µ ohm.cm) 50-90
Hardness (Hv) 450-600
Density (g/cm3) 8.0-8.5
Relative Recoil Permeability (µrec) 1.10
Saturation Field Strength, kOe (kA/m) 37.5 (3000)
Temperature Coefficient of Br (%/°C) -0.05 ~ -0.03
Temperature Coefficient of iHc (%/°C) -0.25 ~ -0.19